Researchers in China have traced a significant share of the degradation seen in copper-plated silicon heterojunction (HJT) solar cells to wear of the screen mesh used to print photoresist, and have proposed a modified screen design to limit the damage. Their study, published in Solar Energy, examined how the printing step affects the sensitive passivating contacts of HJT devices.

Screen printing is a standard metallization technique, but the mechanical pressure and thermal treatment involved can harm passivating structures, increasing recombination and reducing conversion efficiency. The concern is especially acute for copper-plated HJT cells, which are viewed as a promising way to lower metallization costs and cut silver consumption.

Corresponding author Lang Zhou told pv magazine that resist printing differs fundamentally from silver paste printing. With silver paste, screen openings cover only 2–5% of the total area and an emulsion layer shields the rest, keeping the mesh off the wafer. Full-area photoresist coating typically relies on a screen without emulsion so the resist is deposited evenly across the wafer, which means the mesh touches the wafer directly and extensively in every cycle.

Previous work cited by the team recorded efficiency falling from 26.2% to 25.7% across 15,000 consecutive printing cycles in commercial production. Open-circuit voltage and fill factor accounted for most of the loss, while short-circuit current density and electrical resistance stayed largely stable. Minority carrier lifetime degradation climbed from 0.61% with a fresh screen to 11.0% after 15,000 cycles.

Three-dimensional confocal microscopy pointed to gradual wear of the mesh knuckles as the principal cause. As the knuckles wear down, their contact area with the wafer expands, increasing mechanical stress on the passivation stack beneath. Scanning electron microscopy found no visible scratches, but photoluminescence measurements showed higher recombination, indicating damage at the amorphous silicon/crystalline silicon interface.

Balancing protection and uniformity

The team's remedy was an emulsion buffer layer that keeps the mesh from touching the wafer. Six patterns were tested, with emulsion coverage from 2.9% to 16.6%.

Results revealed a trade-off: more emulsion coverage reduced mechanical damage but disrupted ink distribution. A 4.7% coverage ratio gave the best compromise, holding minority carrier lifetime degradation to 0.41% after 10,000 cycles while keeping coating uniformity relatively good. The researchers said the gain stems from the emulsion layer blocking direct mesh–wafer contact and thus limiting cumulative damage to the passivation layers.

Zhou said the findings indicate that a comparatively simple change to screen design can substantially reduce printing-induced degradation and offer a practical route to better manufacturing reliability for copper-plated HJT cells.

The work arrives as copper metallization attracts more attention as a silver substitute in HJT cells. In April 2026, researchers at China's Nankai University reported a silver-free HJT cell at 25.2% efficiency using plasma-induced interface engineering and copper electroplating, tackling adhesion, contact resistance and stability at the ITO interface. Separately, Germany's Forschungszentrum Jülich reached 23.08% with a fully copper-metallized HJT cell, a relatively modest penalty versus its silver-metallized equivalent, while a cell with silver-copper paste on the front and silver contacts on the rear hit 23.95%. Those results highlight copper's potential to curb silver use, although processing and electrical performance still need improvement.